7 Problemau Inc Plastisol Argraffu Sgrin Gyffredin (a Sut i'w Trwsio'n Gyflym)

argraffu sgrin
argraffu sgrin

7 Problemau Inc Plastisol Argraffu Sgrin Gyffredin (a Sut i'w Trwsio'n Gyflym)

Plastisol ink is a thick, colorful ink used to print designs on t-shirts, hats, and other fabrics. But sometimes, things go wrong. This guide will help you fix common plastisol ink problems fast. No confusing words—just simple fixes!


1. Ink Not Sticking to Fabric

Why It Happens

  • Tymheredd halltu is too low (ink needs heat to stick).
  • Fabric has dirt or oils.
  • Cheap ink is used.

How to Fix It

  1. Check the temperature gyda a thermocouple (like a special thermometer).
    • Good temperature: 320°F (160°C) for 30 seconds.
  2. Clean fabric gyda a CCI Chemicals spray before printing.
  3. Use trusted brands like Wilflex neu Rutland inc.

Quick Tip

Fabric Type  Best Temperature
Cotton               320°F (160°C)
Polyester          300°F (149°C)


argraffu sgrin

2. Pinholes or Fisheyes (Tiny Holes in Prints)

Why It Happens

  • Dust on the sgrin.
  • Static electricity (like when clothes stick together).
  • Wrong screen mesh (holes too big).

How to Fix It

  1. Clean screens gyda Ecotex® emulsion remover.
  2. Spray antistatic spray on the fabric.
  3. Defnydd Sefar 110–160 mesh screens.

Astudiaeth Achos

  • Kiwo Squeegees found that antistatic sprays cut pinholes by 40%.

3. Ink Bleeding or Smudging

Why It Happens

  • Too much squeegee pressure.
  • Over-flashing (too much heat between prints).

How to Fix It

  1. Lower squeegee angle to 15–20 degrees.
  2. Defnydd a Xenon flash cure unit to control heat.

Quick Fix Table

Problem                                               Fix
Bleeding colors                     Use FN-INK Quick Cure
Smudged designs                Lower squeegee pressure


4. Tacky or Sticky Prints

Why It Happens

  • Ink is heb ei halltu (not heated enough).
  • Defnyddio phthalate-based plastisol (bad chemicals).

How to Fix It

  1. Check curing with M&R PrintDry sensors.
  2. Switch to Green Galaxy® ink (no bad chemicals).

Fact

  • 65% of shops using phthalate-free ink had fewer sticky prints.

inciau plastisol

5. Ghosting (Double Images)

Why It Happens

  • Screen tension too loose.
  • Wrong squeegee hardness.

How to Fix It

  1. Defnydd a tension meter (aim for 25–30 N/cm²).
  2. Ceisiwch Murakami 70–90 durometer squeegees.

Astudiaeth Achos

  • Switching to 85-durometer squeegees fixed ghosting 80% of the time. 

6. Ink Clogging the Screen

Why It Happens

  • Ink dries too fast.
  • Room is too hot.

How to Fix It

  1. Ychwanegu Union Ink Additives to slow drying.
  2. Work in a cool room (72°F/22°C).

Fact

  • 40% of clogs happen in rooms hotter than 80°F (27°C).

7. Faded Colors

Why It Happens

  • Not enough ink layers.
  • Ink not mixed well.

How to Fix It

  1. Ychwanegu a white underbase layer first.
  2. Mix ink with a Ryonet Mixer.

Quick Tip

Problem                                   Fix
Faded red                      Use 2 layers of ink
Dull colors                     Stir ink for 5 minutes


Pro Tips to Avoid Problems

  1. Defnydd RIP software for perfect color designs.
  2. Store ink in airtight containers.
  3. Test prints with ASTM D4361 wash tests.

Cost Saver

  • Fixing errors early saves $1,200/month

argraffu sgrin

Cwestiynau Cyffredin

Can I mix plastisol with water-based ink? 

No! They don’t work together. Use Matsui water-based ink separately.

How long does plastisol ink last?

6–12 months if stored cool. Rutland ink lasts longest.


Casgliad

Follow these steps to fix plastisol ink problems fast. Check temperatures, clean screens, and use the right tools. 

Rhannu: