{"id":6041,"date":"2025-02-11T01:29:36","date_gmt":"2025-02-11T06:29:36","guid":{"rendered":"https:\/\/plastisol-inks.com\/?p=6041"},"modified":"2025-02-11T01:29:36","modified_gmt":"2025-02-11T06:29:36","slug":"serigrafi-emulsiyonunda-ustalasmak-icin-5-ipucu","status":"publish","type":"post","link":"https:\/\/plastisol-inks.com\/tr\/5-tips-for-mastering-screen-printing-emulsion\/","title":{"rendered":"Serigrafi Em\u00fclsiyonunda Uzmanla\u015fmak \u0130\u00e7in 5 G\u00fc\u00e7l\u00fc \u0130pucu"},"content":{"rendered":"<p>K\u00fcrleme, kaplama ve kusurlar\u0131 tespit etme konusunda 5 g\u00fc\u00e7l\u00fc ipucuyla serigrafi em\u00fclsiyonunda ustala\u015f\u0131n. Her seferinde kusursuz bask\u0131lar elde edin.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">1.<strong>Serigrafi Bask\u0131da A\u015f\u0131r\u0131 Pozlaman\u0131n Belirtileri<\/strong><br><\/h3>\n\n\n\n<p>Em\u00fclsiyon k\u00fcrleme i\u015flemi s\u0131ras\u0131nda a\u015f\u0131r\u0131 pozlama, yeni ba\u015flayanlar i\u00e7in s\u0131k kar\u015f\u0131la\u015f\u0131lan bir sorundur. A\u015f\u0131r\u0131 pozlaman\u0131n temel g\u00f6stergeleri \u015funlard\u0131r:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>\u015eablonlar\u0131n bask\u0131 s\u0131ras\u0131nda k\u0131r\u0131lganla\u015fmas\u0131 ve \u00e7atlamas\u0131.<\/li>\n\n\n\n<li>Uzun s\u00fcreli durulamadan sonra bile, maruz kalmayan em\u00fclsiyonun y\u0131kanmas\u0131nda zorluk.<\/li>\n\n\n\n<li>A\u015f\u0131r\u0131 UV sertle\u015ftirmesi nedeniyle ince detaylar\u0131n kayb\u0131.<\/li>\n\n\n\n<li>Filmin kenarlar\u0131nda \u0131\u015f\u0131\u011f\u0131n s\u0131zd\u0131\u011f\u0131 yerlerde g\u00f6zle g\u00f6r\u00fcl\u00fcr &quot;g\u00f6lgelenme&quot; vard\u0131.<\/li>\n<\/ul>\n\n\n\n<p>A\u015f\u0131r\u0131 maruziyeti \u00f6nlemek i\u00e7in, her zaman bir pozlama hesaplay\u0131c\u0131s\u0131 kullanarak bir pozlama testi yap\u0131n ve em\u00fclsiyon tipine g\u00f6re UV \u0131\u015f\u0131k mesafesini ve zamanlamas\u0131n\u0131 ayarlay\u0131n.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\"><strong>Nedir <a href=\"https:\/\/plastisol-inks.com\/tr\/emulsiyon-7-temel-faktor-serigrafi-baski\/\" data-type=\"link\" data-id=\"https:\/\/plastisol-inks.com\/emulsion-7-key-factors-screen-printing\/\">Serigrafi Bask\u0131 Em\u00fclsiyonu<\/a>?<\/strong><br><\/h3>\n\n\n\n<p>Serigrafi em\u00fclsiyonu, m\u00fcrekkep transferi i\u00e7in \u015fablonlar olu\u015fturmak \u00fczere a\u011f ekranlar\u0131na uygulanan \u0131\u015f\u0131\u011fa duyarl\u0131 bir s\u0131v\u0131d\u0131r. UV \u0131\u015f\u0131\u011f\u0131na maruz kald\u0131\u011f\u0131nda sertle\u015ferek, m\u00fcrekkebin tasar\u0131m d\u0131\u015f\u0131 alanlarda bloke olmas\u0131n\u0131 sa\u011flarken a\u00e7\u0131k a\u011f b\u00f6l\u00fcmlerinden ge\u00e7mesine izin verir.<\/p>\n\n\n\n<p>\u0130ki ana t\u00fcr\u00fc vard\u0131r:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>\u00c7ift-K\u00fcr Em\u00fclsiyonlar\u0131<\/strong>: Detayl\u0131 i\u015fler i\u00e7in idealdir; daha fazla \u00e7ok y\u00f6nl\u00fcl\u00fck i\u00e7in diazo ve fotopolimeri birle\u015ftirir.<\/li>\n\n\n\n<li><strong>Fotopolimer Em\u00fclsiyonlar<\/strong>: Daha h\u0131zl\u0131 pozlama s\u00fcreleriyle bilinir, ancak a\u015f\u0131r\u0131 pozlama konusunda daha az affedicidir.<\/li>\n<\/ul>\n\n\n\n<p>Yeni ba\u015flayanlar i\u00e7in Ulano QTX veya Chromablue gibi \u00e7ift k\u00fcrl\u00fc em\u00fclsiyonlar kullan\u0131m kolayl\u0131\u011f\u0131 ve performans aras\u0131nda m\u00fckemmel bir denge sunar.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">3.<strong>Ka\u00e7 Kat Em\u00fclsiyon Uygulamal\u0131s\u0131n\u0131z?<\/strong><br><\/h3>\n\n\n\n<p>\u00c7o\u011fu ekran, her taraf i\u00e7in 1-2 kat, toplamda 2-4 kat gerektirir. Kat say\u0131s\u0131 \u015funlara ba\u011fl\u0131d\u0131r:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>\u00d6rg\u00fc Say\u0131s\u0131<\/strong>:Daha y\u00fcksek g\u00f6zenek say\u0131lar\u0131 (\u00f6rne\u011fin 230+) t\u0131kanmay\u0131 \u00f6nlemek i\u00e7in daha ince katlar gerektirir.<\/li>\n\n\n\n<li><strong>Em\u00fclsiyon Viskozitesi<\/strong>:Daha kal\u0131n em\u00fclsiyonlar genellikle daha az kat gerektirir.<\/li>\n<\/ul>\n\n\n\n<p><strong>Profesyonel \u0130pucu<\/strong>: E\u015fit em\u00fclsiyon uygulamas\u0131 i\u00e7in bir kep\u00e7e kaplay\u0131c\u0131 kullan\u0131n. Ekran\u0131 45\u00b0 a\u00e7\u0131yla tutun, em\u00fclsiyonu d\u00fczg\u00fcn, yukar\u0131 do\u011fru hareketlerle uygulay\u0131n ve bir sonrakini eklemeden \u00f6nce her kat\u0131n tamamen kurumas\u0131n\u0131 bekleyin (30\u201360 dakika).<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">4.<strong>K\u00f6t\u00fc Em\u00fclsiyon Nas\u0131l Belirlenir<\/strong><br><\/h3>\n\n\n\n<p>Son kullanma tarihi ge\u00e7mi\u015f veya bozulmu\u015f em\u00fclsiyon ba\u015far\u0131s\u0131z \u015fablonlara yol a\u00e7abilir. Em\u00fclsiyonunuzun art\u0131k kullan\u0131lamaz oldu\u011funa dair i\u015faretler \u015funlard\u0131r:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>Renk De\u011fi\u015fimleri<\/strong>: Sar\u0131 veya kahverengi tonlar kimyasal par\u00e7alanmay\u0131 d\u00fc\u015f\u00fcnd\u00fcr\u00fcr.<\/li>\n\n\n\n<li><strong>Topakl\u0131 Doku<\/strong>: P\u00fcr\u00fczs\u00fcz bir em\u00fclsiyon idealdir; topaklar bozulman\u0131n g\u00f6stergesidir.<\/li>\n\n\n\n<li><strong>Zay\u0131f Yap\u0131\u015fma<\/strong>: E\u011fer em\u00fclsiyon y\u0131kama esnas\u0131nda soyulursa, fotosensitivite \u00f6zelli\u011fini kaybetmi\u015f demektir.<\/li>\n\n\n\n<li><strong>K\u00f6t\u00fc Koku<\/strong>: Ek\u015fi bir koku bakteri olu\u015fumunu akla getirir.<\/li>\n<\/ul>\n\n\n\n<p>Son kullanma tarihini mutlaka kontrol edin ve em\u00fclsiyonu serin ve karanl\u0131k bir yerde saklay\u0131n.<\/p>\n\n\n\n<figure class=\"wp-block-image aligncenter size-full\"><img fetchpriority=\"high\" decoding=\"async\" width=\"800\" height=\"800\" src=\"https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-6_\u526f\u672c.jpg\" alt=\"Serigrafi Bask\u0131 Em\u00fclsiyonu\" class=\"wp-image-6046\" title=\"plastisol m\u00fcrekkepler\" srcset=\"https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-6_\u526f\u672c.jpg 800w, https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-6_\u526f\u672c-300x300.jpg 300w, https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-6_\u526f\u672c-150x150.jpg 150w, https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-6_\u526f\u672c-768x768.jpg 768w, https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-6_\u526f\u672c-100x100.jpg 100w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><figcaption>plastisol m\u00fcrekkepler<\/figcaption><\/figure>\n\n\n\n<h3 class=\"wp-block-heading\">5.<strong>Ne Kadar S\u00fcrer? <a href=\"https:\/\/plastisol-inks.com\/tr\/serigrafi-baski-murekkebinin-hassasiyeti\/\" data-type=\"link\" data-id=\"https:\/\/plastisol-inks.com\/the-precision-of-silk-screen-printing-ink\/\">Em\u00fclsiyon<\/a> Tedavi etmek i\u00e7in mi?<\/strong><br><\/h3>\n\n\n\n<p>Bir kez kaplan\u0131p kurutulduktan sonra, em\u00fclsiyonun tamamen k\u00fcrlenmesi i\u00e7in UV maruziyeti gerekir. K\u00fcrlenme s\u00fcreleri em\u00fclsiyon t\u00fcr\u00fcne g\u00f6re de\u011fi\u015fir:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>\u00c7ift-K\u00fcr Em\u00fclsiyonu<\/strong>: 500W UV \u0131\u015f\u0131k alt\u0131nda 3\u20138 dakika.<\/li>\n\n\n\n<li><strong>Fotopolimer Em\u00fclsiyon<\/strong>: 1\u20133 dakika.<\/li>\n<\/ul>\n\n\n\n<p>Pozlamadan sonra, em\u00fclsiyonun sabitlenmesi i\u00e7in y\u0131kamadan \u00f6nce ekran\u0131 15-30 dakika dinlendirin.<\/p>\n\n\n\n<h3 class=\"wp-block-heading\">6.<strong>Serigrafi Bask\u0131 Em\u00fclsiyonunun Raf \u00d6mr\u00fc<\/strong><br><\/h3>\n\n\n\n<p>Kar\u0131\u015ft\u0131r\u0131lmam\u0131\u015f serigrafi bask\u0131 em\u00fclsiyonu, uygun \u015fekilde sakland\u0131\u011f\u0131nda 6-12 ay dayanabilir. \u00c7ift k\u00fcrleme em\u00fclsiyonlar\u0131 i\u00e7in diazo ile kar\u0131\u015ft\u0131r\u0131ld\u0131\u011f\u0131nda, 2-3 ay i\u00e7inde kullan\u0131n.<\/p>\n\n\n\n<p><strong>Raf \u00f6mr\u00fcn\u00fc uzatmak i\u00e7in<\/strong>:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li>A\u00e7\u0131lmam\u0131\u015f ambalajlar\u0131 buzdolab\u0131nda saklay\u0131n\u0131z.<\/li>\n\n\n\n<li>Temiz aletler kullanarak kirlenmeyi \u00f6nleyin.<\/li>\n\n\n\n<li>Kullan\u0131mdan sonra kaplar\u0131 s\u0131k\u0131ca kapat\u0131n.<\/li>\n<\/ul>\n\n\n\n<h3 class=\"wp-block-heading\">7.<strong>Nas\u0131l D\u00fczeltilir <a href=\"https:\/\/plastisolink.us\/tape-for-screens-repair-solutions-for-displays\/\" data-type=\"link\" data-id=\"https:\/\/plastisolink.us\/tape-for-screens-repair-solutions-for-displays\/\" rel=\"nofollow noopener\" target=\"_blank\">A\u015f\u0131r\u0131 pozlama<\/a> Serigrafi Bask\u0131da<\/strong><\/h3>\n\n\n\n<p>Ekran\u0131n\u0131zda a\u015f\u0131r\u0131 pozlamay\u0131 tespit etti\u011finizde, daha fazla bask\u0131ya ge\u00e7meden \u00f6nce bunu d\u00fczeltmeniz \u00f6nemlidir. A\u015f\u0131r\u0131 pozlanm\u0131\u015f ekranlarla ba\u015fa \u00e7\u0131kman\u0131n birka\u00e7 yolu \u015funlard\u0131r:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>Y\u0131kama S\u00fcresini Art\u0131r\u0131n<\/strong>: E\u011fer a\u00e7\u0131\u011fa \u00e7\u0131kmam\u0131\u015f em\u00fclsiyonu y\u0131kayam\u0131yorsan\u0131z, uzun bir s\u00fcre boyunca hafif\u00e7e \u00e7alkalayarak \u0131l\u0131k su kullanmay\u0131 deneyin. Sab\u0131rl\u0131 olun, \u00e7\u00fcnk\u00fc bu em\u00fclsiyonun yumu\u015famas\u0131n\u0131 ve a\u011fdan ayr\u0131lmas\u0131n\u0131 sa\u011flayacakt\u0131r.<\/li>\n\n\n\n<li><strong>Ekran\u0131 yeniden kaplay\u0131n<\/strong>: E\u011fer a\u015f\u0131r\u0131 pozlama \u015fablonu tehlikeye att\u0131ysa, ekrana tekrar em\u00fclsiyon uygulaman\u0131z gerekebilir. A\u015f\u0131r\u0131 pozlama \u015fablonunu \u00e7\u0131kard\u0131ktan sonra, a\u011f\u0131 iyice temizleyin, ard\u0131ndan tekrar taze em\u00fclsiyonla kaplay\u0131n.<\/li>\n\n\n\n<li><strong>Sonraki Bask\u0131lar \u0130\u00e7in Pozlama S\u00fcresini Azalt\u0131n<\/strong>: Gelecekteki bask\u0131larda ayn\u0131 sorunu ya\u015famamak i\u00e7in pozlama s\u00fcresini biraz azalt\u0131n veya pozlama s\u0131ras\u0131nda ekran ile UV \u0131\u015f\u0131k kayna\u011f\u0131 aras\u0131ndaki mesafeyi azalt\u0131n. Ayarlar\u0131 ince ayarlamak i\u00e7in test pozlamalar\u0131 ger\u00e7ekle\u015ftirin.<\/li>\n<\/ul>\n\n\n\n<h3 class=\"wp-block-heading\">8.Serigrafi Bask\u0131da Ar\u0131zalar\u0131n Giderilmesi<\/h3>\n\n\n\n<p>Em\u00fclsiyon k\u00fcrlemede ustala\u015fmak \u00e7ok \u00f6nemli olsa da, yayg\u0131n bask\u0131 kusurlar\u0131 yine de meydana gelebilir. \u0130\u015fte bunlar\u0131 nas\u0131l giderece\u011finiz:<\/p>\n\n\n\n<ul class=\"wp-block-list\">\n<li><strong>\u0130\u011fne delikleri<\/strong>: Bask\u0131lar\u0131n\u0131zdaki minik, yuvarlak delikler genellikle ekrandaki kirlenmeden veya uygunsuz \u015fekilde kaplanm\u0131\u015f bir \u015fablondan kaynaklan\u0131r. Kaplamadan \u00f6nce ekran\u0131n\u0131z\u0131n iyice temizlendi\u011finden emin olun ve pozlamadan \u00f6nce toz veya kal\u0131nt\u0131 olup olmad\u0131\u011f\u0131n\u0131 kontrol edin.<\/li>\n\n\n\n<li><strong>Bulan\u0131k Bask\u0131lar<\/strong>: Bu, \u015fablon d\u00fczg\u00fcn bir \u015fekilde pozland\u0131r\u0131lmam\u0131\u015fsa veya k\u00fcrlenmemi\u015fse meydana gelebilir. \u015eablon \u00e7ok yumu\u015faksa veya pozlama yetersizse, ince ayr\u0131nt\u0131lar silinebilir veya bulan\u0131k g\u00f6r\u00fcnebilir. Do\u011fruluk i\u00e7in her zaman bir test pozlamas\u0131 ger\u00e7ekle\u015ftirin.<\/li>\n\n\n\n<li><strong>D\u00fczensiz M\u00fcrekkep Kapsam\u0131<\/strong>: Bu genellikle uygunsuz bir sonucun sonucudur<a href=\"https:\/\/plastisolink.us\/screen-cure-mastering-perfect-screen-prints\/\" data-type=\"link\" data-id=\"https:\/\/plastisolink.us\/screen-cure-mastering-perfect-screen-prints\/\" rel=\"nofollow noopener\" target=\"_blank\"> em\u00fclsiyon kaplama<\/a> veya bask\u0131 s\u0131ras\u0131nda e\u015fit olmayan bas\u0131n\u00e7. Em\u00fclsiyon uygulamas\u0131n\u0131 kontrol edin ve ekran\u0131n\u0131z\u0131n temiz ve iyi haz\u0131rlanm\u0131\u015f oldu\u011fundan emin olun.<\/li>\n<\/ul>\n\n\n\n<h3 class=\"wp-block-heading\">9.<strong>Em\u00fclsiyon ve Ekranlar\u0131n\u0131z\u0131n Bak\u0131m\u0131<\/strong><\/h3>\n\n\n\n<p>Hem em\u00fclsiyonunuzun hem de ekranlar\u0131n\u0131z\u0131n uygun \u015fekilde bak\u0131m\u0131, \u00f6m\u00fcrlerini uzatman\u0131za ve bask\u0131 kalitesini art\u0131rman\u0131za yard\u0131mc\u0131 olacakt\u0131r. M\u00fcrekkep kal\u0131nt\u0131s\u0131 birikmesini \u00f6nlemek i\u00e7in ekranlar\u0131n\u0131z\u0131 d\u00fczenli olarak ekran temizleme kimyasallar\u0131yla temizleyin ve ekranlar\u0131 do\u011frudan g\u00fcne\u015f \u0131\u015f\u0131\u011f\u0131ndan uzak, serin ve kuru bir yerde dik olarak saklay\u0131n.<\/p>\n\n\n\n<p>Do\u011fru \u015fekilde y\u00f6netilen ekranlar ve em\u00fclsiyonlar bask\u0131lar\u0131n\u0131z\u0131n tutarl\u0131l\u0131\u011f\u0131 ve kalitesinde \u00f6nemli bir fark yarat\u0131r, bu nedenle bak\u0131m ad\u0131mlar\u0131n\u0131 asla atlamay\u0131n.<\/p>\n\n\n\n<figure class=\"wp-block-image aligncenter size-full\"><img decoding=\"async\" width=\"750\" height=\"1000\" src=\"https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-4_\u526f\u672c.jpg\" alt=\"Serigrafi Bask\u0131 Em\u00fclsiyonu\" class=\"wp-image-6047\" title=\"plastisol m\u00fcrekkepler\" srcset=\"https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-4_\u526f\u672c.jpg 750w, https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-4_\u526f\u672c-225x300.jpg 225w\" sizes=\"(max-width: 750px) 100vw, 750px\" \/><figcaption>plastisol m\u00fcrekkepler<\/figcaption><\/figure>\n\n\n\n<h3 class=\"wp-block-heading\">Sonu\u00e7<\/h3>\n\n\n\n<p>Serigrafi bask\u0131 em\u00fclsiyonunda ustala\u015fmak, keskin ve dayan\u0131kl\u0131 bask\u0131lar \u00fcretmek i\u00e7in olmazsa olmazd\u0131r. A\u015f\u0131r\u0131 pozlamay\u0131 \u00f6nlemekten son kullanma tarihi ge\u00e7mi\u015f em\u00fclsiyonu tespit etmeye kadar, bu uzman ipu\u00e7lar\u0131 i\u015f ak\u0131\u015f\u0131n\u0131z\u0131 kolayla\u015ft\u0131rman\u0131za yard\u0131mc\u0131 olacakt\u0131r. Uygun depolama, hassas kaplama ve d\u00fczenli testlere \u00f6ncelik vererek, her seferinde bask\u0131 sonu\u00e7lar\u0131n\u0131z\u0131 en \u00fcst d\u00fczeye \u00e7\u0131karabilirsiniz.<\/p>\n\n\n\n<figure class=\"wp-block-image aligncenter size-full\"><img decoding=\"async\" width=\"900\" height=\"383\" src=\"https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-8_\u526f\u672c.jpg\" alt=\"plastisol m\u00fcrekkepler\" class=\"wp-image-6044\" title=\"plastisol m\u00fcrekkepler\" srcset=\"https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-8_\u526f\u672c.jpg 900w, https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-8_\u526f\u672c-300x128.jpg 300w, https:\/\/plastisol-inks.com\/wp-content\/uploads\/2025\/02\/images-8_\u526f\u672c-768x327.jpg 768w\" sizes=\"(max-width: 900px) 100vw, 900px\" \/><figcaption>plastisol m\u00fcrekkepler<\/figcaption><\/figure>","protected":false},"excerpt":{"rendered":"<p>Master screen printing emulsion with 5 powerful tips on curing, coating, and spotting defects. Ensure flawless prints every time . 1.Signs of Overexposure in Screen Printing Overexposure during the emulsion curing process is a frequent issue for beginners. Key indicators of overexposure include: To prevent overexposure, always perform an exposure test using an exposure calculator, [&hellip;]<\/p>\n","protected":false},"author":2,"featured_media":6045,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"disabled","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-gradient":""}},"footnotes":""},"categories":[1],"tags":[159],"class_list":["post-6041","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-blog","tag-screen-printing-emulsion"],"_links":{"self":[{"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/posts\/6041","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/users\/2"}],"replies":[{"embeddable":true,"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/comments?post=6041"}],"version-history":[{"count":3,"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/posts\/6041\/revisions"}],"predecessor-version":[{"id":6048,"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/posts\/6041\/revisions\/6048"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/media\/6045"}],"wp:attachment":[{"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/media?parent=6041"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/categories?post=6041"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/plastisol-inks.com\/tr\/wp-json\/wp\/v2\/tags?post=6041"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}